Research Article

Conductivity at Low Humidity of Materials Derived from Ferroxane Particles

Figure 3

XRD diffractograms of pellets sintered for 4 hours at: (a) 300°C, (b) 500°C. The peak at 2 = 44.2° is due to the sample holder.