Research Article
The Corrosion Behaviour of WC-Co-Ru Alloys in Aggressive Chloride Media
Table 3
Electrochemical parameters for the investigated alloys in 1 M sodium chloride.
| Sample (wt% Ru) | (V) | (A) ×10−6 | (A/m2) ×10−3 | (A/m2) ×10−4 | (V/Dec) | (V/Dec) | CR (mm/a) ×10−2 |
| 0.0 | −0.280 | 190 | 7.89 | 3.79 | 0.016 | 0.039 | 350 | 0.4 | −0.301 | 0.36 | 14.3 | 35.1 | 0.038 | 0.028 | 0.65 | 1.0 | −0.258 | 0.90 | 35.6 | 513 | 0.039 | 0.029 | 1.62 | 1.5 | −0.483 | 0.62 | 51.3 | 76.3 | 0.078 | 0.029 | 1.11 | 2.0 | −0.275 | 0.16 | 0.99 | 3.36 | 0.051 | 0.021 | 0.28 | 3.0 | −0.220 | 0.11 | 0.31 | 1.43 | 0.027 | 0.022 | 0.21 |
|
|