Microhardness values of prepared coating samples.
| Samples | Microhardness HV 0.3, 15s |
| NA4 | 315 ± 31 |
| NA5 | 284 ± 22 |
| NA6 | 258 ± 32 |
| NA8 | 255 ± 33 |
| NA10 | 280 ± 22 |
| NC4 | 275 ± 29 |
| NC5 | 266 ± 23 |
| NC6 | 274 ± 31 |
| NC8 | 292 ± 43 |