Ground Penetrating Radar Assessment of Flexible Road Pavement Degradation

Figure 1

Structural defects investigated in this study: (a) longitudinal and transverse cracks, (b) longitudinal cracks only, (c) transverse cracks only, (d) ramified cracks, and (e) failures. The half road pavement is about 3 m.