Research Article
Development of Combinatorial Pulsed Laser Deposition for Expedited Device Optimization in CdTe/CdS Thin-Film Solar Cells
Figure 6
The values of open circuit voltage (a), short circuit current (b), fill factor (c), and efficiency (d) as a function of CdTe thickness for sample A made without any CdCl2 annealing and sample B3 that underwent a 15 min CdCl2 annealing.
(a) versus thickness |
(b) versus thickness |
(c) Fill factor versus thickness |
(d) Efficiency versus thickness |