Efficiencies for five samples processed at different CdCl2 annealing times.

Layer thicknessNo CdCl210min.12min.15min.17min.

Layer 1 (1.5 μm)0.081.732.394.462.90
Layer 2 (1.25 μm)0.121.954.354.793.51
Layer 3 (1.0 μm)0.132.304.545.093.99
Layer 4 (0.75 μm)0.152.955.165.344.08