Absorption peaks from Sm2O3-doped Na2O–ZnO–P2O5 glasses and their excitation levels, ground state 6H5/2 →.

Peaks / nmExcited state

3674D1/2 + 4P7/2
4056P5/2, 4K11/2
4724I1/2+ 4I13/2+4M15/2
9506F11/2
10386F9/2
12386F7/2
13856F5/2
14896F3/2
15526F1/2
16236H15/2