Research Article

Durability of Ag- T i O 2 Photocatalysts Assessed for the Degradation of Dichloroacetic Acid

Figure 3

(a) Degradation of DCA (shown as release of H + ) using the photocatalyst 0.35 Ag- T i O 2 at pH 3 in 3 consecutive runs, 1st run (—), 2nd run ( - - - ), 3rd run ( ), a 3rd run (- -) with addition of 4 mM C l before the run started, and slope (280513.fig.001xxx) used for the determination of the photonic efficiency of each run with 𝐼 3 . 3 9 × 1 0 2 Einstein L 1 h 1 . The photocatalyst loading was 0.5 g/L. (b) Degradation of DCA (shown as release of H + ) using the photocatalyst 0.35 Ag- T i O 2 at pH 3 in 3 consecutive runs with intermittent washing between runs, 1st run (—), 2nd run ( - - - ), 3rd run ( ), and slope (280513.fig.001xxx) used for the determination of the photonic efficiency with 𝐼 3 . 3 9 × 1 0 2 Einstein L 1 h 1 . The photocatalyst loading was 0.5 g/L.
280513.fig.003a
(a)
280513.fig.003b
(b)