Research Article

Preparation of Fluorine-Doped TiO2 Photocatalysts with Controlled Crystalline Structure

Figure 4

Pore size distribution in the undoped TiO2 calcinated at different temperatures (a) and in the TF10 and TF20 powders calcinated at 400°C (b).
534038.fig.004a
(a)
534038.fig.004b
(b)