Research Article

/ Composite Films Immobilized on Foam Nickel Substrate for the Photocatalytic Degradation of Gaseous Acetaldehyde

Figure 6

FE-SEM images of bare-foam nickel (a), S2 (b), and S2T2 (c). The scale is 200  m.
679421.fig.006a
(a)
679421.fig.006b
(b)
679421.fig.006c
(c)