Table 2

Comparison of and the summation of for each loading ratio of TiO2.

F (—) (—)

Loading ratio of TiO2 (wt%) α

1 −0.60 −0.87 −0.29 −1.76
100.0270.110.0450.18
150.230.75 −0.13 0.85
200.760.480.671.91
300.350.890.291.53
600.310.310.110.73
80 −0.35 −0.66 −0.25 −1.26