Review Article

Achievements and Challenges of CdS/CdTe Solar Cells

Figure 3

AFM of (a) standard CBD CdS with roughness of 12.2 nm, (b) CBD CdS with CdCl2 annealing treatment at 300°C with roughness of 14.6 nm, (c) bilayer CdS with total 80 nm thickness with roughness of 7.2 nm. Figures are taken from [30].
297350.fig.003a
(a)
297350.fig.003b
(b)