Effect of catalyst concentration on photocatalytic degradation of aniline under UV illumination in HCBR (experimental conditions: initial aniline: 50 mg/L; initial pH: 6, temperature: 293 K).

Catalyst concentration (mg/L)Equation 𝐾 a p 𝑅 2

0 (only UV)0.061x + 0.1780.0610.97
200.066x + 0.1780.0660.897
400.132x + 0.3110.1320.988
600.265x + 0.3970.2650.939