Research Article
Low Cost Amorphous Silicon Intrinsic Layer for Thin-Film Tandem Solar Cells
Table 2
The results of modulates fabricated with these three kinds of amorphous silicon intrinsic layer.
| Condition (FR, P, Pw, Dilu) | SiH4 consumption | Tact time (s) | Initial module power (W) |
| 20.8, 0.5, 380, 1 | 100.00% | 835 | 138.85 | 15.6, 0.5, 380, 2.5 | 102.60% | 1076 | 138.57 | 20.8, 0.5, 340, 3 (original) | 182.00% | 1400 | 138.75 |
|
|