Research Article
Photocatalytic Degradation of Methyl Violet with TiSiW12O40/TiO2
Table 1
Comparison of photocatalytic activity of catalysts.
| Type of catalyst | Catalyst dosage | Reaction conditions | Degradation rate |
| Co-SBA-15 | 1 g/L | Initial concentration 50 mg/L, within 150 min of solar light irradiation | 61% | Fe-doped anatase TiO2 | 0.18 g | Initial concentration 4 mg/L, pH is 5.5, within 4 h visible light | 59.4% | TiO2 | 0.3 g | Initial concentration 20 mg/L, pH is 5.5, within 3 h simulated natural light irradiation | 58.8% | H4SiW12O40 | 0.3 g | Initial concentration 20 mg/L, pH is 5.5, within 3 h simulated natural light irradiation | 21.5% | TiSiW12O40/TiO2 | 0.3 g | Initial concentration 20 mg/L, pH is 5.5, within 3 h simulated natural light irradiation | 82.4% |
|
|