Research Article

H2O2 Treatment of Electrochemically Deposited Cu2O Thin Films for Enhancing Optical Absorption

Figure 1

(a) SEM images of the as-deposited film. (b) SEM images of the film treated at room temperature for 7 hours. (c) and (d) SEM images of the film treated at room temperature for 24 hours (with different magnifications).
738063.fig.001a
(a)
738063.fig.001b
(b)
738063.fig.001c
(c)
738063.fig.001d
(d)