Photocatalytic Decolourization of Direct Yellow 9 on Titanium and Zinc Oxides

Table 1

Pseudofirst-order rate constants and half-live times for photocatalytic degradation of DY9 upon irradiation with solar simulated light (500 W/m2) at varying DY9 concentration.

DY9 concentration/ mol·L−1TiO2 (1.5 g·L−1)ZnO (1.5 g·L−1)
/min−1 /min /min−1 /min

100.075890.09897
300.0314220.066910
500.0312220.049114
800.0226310.030023
1000.0180390.025028