Optical, Electrical and Photocatalytic Properties of the Ternary Semiconductors , and
Figure 2
(a) X-ray diffraction patterns of the ternary semiconductor compounds annealed at 250°C (bottom patterns) and 450°C (top patterns) of (A) and (B) . (b) X-ray diffraction patterns of the ternary semiconductor compounds of , (A) as a function of annealing temperature and (B) zoom in of the peaks (002) to observe the shift.