Research Article

Investigation on Thermal Degradation Process of Polymer Solar Cells Based on Blend of PBDTTT-C and BM

Figure 8

TEM images of the PBDTTT-C: PC70BM films treated at 70°C for control (a), 1 hour (b), 2 hours (c), 3 hours (d), 5 hours (e), and 18 hours (f).
354837.fig.008a
(a)
354837.fig.008b
(b)
354837.fig.008c
(c)
354837.fig.008d
(d)
354837.fig.008e
(e)
354837.fig.008f
(f)