Table 1: The spin coating parameters of NDPs films for each factor and level as defined by the Taguchi experiment design.

ParametersSample 1Sample 2Sample 3

Spin speed (rpm)250035005500
Spin time (sec.)303030
Heat treatment (°C)300300300