Research Article
Self-Assembly of TiO2/CdS Mesoporous Microspheres with Enhanced Photocatalytic Activity via Hydrothermal Method
Table 1
BET surface area and pore volume of the as-synthesized samples.
| Sample | TiO2 (wt.%) | Time (h)
| S
BET (m2/g) | Pore volume (cm3/g) |
| CdS | 0 | 10
| 25.4 | 0.07 | TiO2/CdS | 10 | 10 | 54.9 | 0.16 | TiO2/CdS | 12 | 10 | 62.7 | 0.14 | TiO2/CdS | 7 | 10 | 47.3 | 0.12 | TiO2/CdS | 10 | 20 | 57.2 | 0.15 | TiO2/CdS | 10 | 5 | 51.0 | 0.13 |
|
|