Research Article
Optimization of Solar Module Encapsulant Lamination by Optical Constant Determination of Ethylene-Vinyl Acetate
Figure 8
(a) The refractive index and optical transmittance of EVA versus the lamination time at a fixed lamination temperature of 150°C. (b) The refractive index and optical transmittance of EVA as functions of the lamination temperature for a fixed lamination time of 7 minutes.
(a) |
(b) |