Research Article

Synthesis, Analysis, and Testing of BiOBr-Bi2WO6 Photocatalytic Heterojunction Semiconductors

Figure 14

Degradation efficiency versus irradiation time by utilizing photocatalysts hydrothermally synthesized and mechanically mixed (ratio of BiOBr to Bi2WO6: 1 : 1; catalysts dosage: 0.5 g/L; temperature: ()°C; pH = 5; and initial concentration: 10 ppm).