Research Article

Synthesis and Characterization of Graphene Oxide-Modified Bi2WO6 and Its Use as Photocatalyst

Figure 4

(a) Adsorption capacity of RhB on pure Bi2WO6, 1.2% G-BWO, and GO. (b) Degradation curves of RhB in the presence of different prepared samples under visible light irradiation (catalysts dosage amount: 1 g/L; co = 10 ppm; T = 20°C).
(a)
(b)