Device 5 finger 2 time-dependent voltage degradation.

Light intensity (mW/cm2)ExperimentIsc (mA/cm2)Voc (mV)FFVmp (mV)Imp (mA/cm2)Efficiency (%)Power losses (%)

100After manufacture5,0475800,5194203,6201,520
Initial5,7925600,4964004,1201,648
After 10 V 2 min5,7675200,3913403,4451,17128,926
After 10 V 3 min5,8265200,3813203,6111,1551,347
After 10 V 10 min5,6864900,3803003,5331,0608,278
After 15 V 20 min3,6874800,3783003,4361,0312,731
After 15 V 30 min5,5224800,3643003,2180,9666,355
After 15 V 40 min5,5194700,3572903,2010,9283,844
50After voltage degradation3,3444000,3262401,8170,872
302,2363400,3072001,1660,777
101,7463000,2971600,9731,557
10,8221800,2781000,4124,123