Research Article
Experimental Analysis of the Potential Induced Degradation Effect on Organic Solar Cells
Table 8
Device 3 finger 4 air and O2 plasma degradation.
| Light intensity | Experiment | Isc (mA/cm2) | Voc (mV) | FF | Vmp (mV) | Imp (mA/cm2) | Efficiency (%) | Power losses (%) |
| 100 mW/cm2 | Initial | 8,418 | 580 | 0,536 | 420 | 6,227 | 2,615 | — | 8 min air | 7,636 | 580 | 0,512 | 400 | 5,671 | 2,268 | 13,264 | 6 min O2 plasma | 7,364 | 560 | 0,526 | 400 | 5,425 | 2,170 | 4,343 |
|
|