Research Article

Characteristics of Nanocrystallite-CdS Produced by Low-Cost Electrochemical Technique for Thin Film Photovoltaic Application: The Influence of Deposition Voltage

Table 5

Percentage Cd and S atomic compositions of as-deposited and annealed CdS samples grown for 45 minutes at different cathodic voltages.

Cathodic growth voltage
(mV)
Growth time
(min)
Atomic composition (%)As-deposited
Cd/S
Annealed
Cd/S
As-depositedAnnealed
CdSCdS

14454546.653.446.753.30.870.88
14504546.653.447.852.20.870.92
14554546.653.447.852.20.870.92
14604545.154.945.754.30.820.84
14654542.157.944.255.80.730.79