3D images (0 < x < 1280 μm; 0 < y < 960 μm; z variable) obtained from surface samples analyzed with confocal laser scanning microscope: (a) mortar W/C = 0.4, 600 steps of 2 μm with an optical zoom x10, (b) mortar W/C = 0.5, 250 steps of 1 μm with an optical zoom x10, and (c) wood, 200 steps of 1 μm with an optical zoom x5.
(a)
(b)
(c)