Research Article
Investigation on Parameters Affecting the Effectiveness of Photocatalytic Functional Coatings to Degrade NO: TiO2 Amount on Surface, Illumination, and Substrate Roughness
Figure 9
Influence of TiO2 dry matter content applied to surface (in g/m2) on NO degradation ratio (in %) for each substrate under three different illumination conditions (the NO2 generation is also represented): (a) mortar W/C = 0.4, (b) mortar W/C = 0.5, and (c) wood.
(a) |
(b) |
(c) |