Research Article
A Solution-Processed Tetra-Alkoxylated Zinc Phthalocyanine as Hole Transporting Material for Emerging Photovoltaic Technologies
Table 3
Average values of the main photovoltaic characteristics of (n-BuO)4ZnPc and Spiro-OMeTAD.
| HTM | (V) | (mA/cm2) | (%) | (%) |
| (n-BuO)4ZnPc | Forward bias | 0.896 ± 0.009 | 12.1 ± 1.2 | 57.0 ± 3.1 | 6.06% ± 0.74 | Reverse bias | 0.928 ± 0.04 | 14.5 ± 1.9 | 61.8 ± 2.6 | 9.00% ± 0.21 | Spiro-OMeTAD | Forward bias | 0.903 ± 0.02 | 13.6 ± 0.9 | 55.2 ± 4.0 | 6.75% ± 0.19 | Reverse bias | 0.928 ± 0.04 | 14.5 ± 1.9 | 61.8 ± 2.6 | 8.61% ± 0.60 |
|
|