Research Article
Investigation on Potential-Induced Degradation in a 50 MWp Crystalline Silicon Photovoltaic Power Plant
Figure 8
The I-V and P-V curves of solar modules disassembled from the same PID-affected module string in the power plant under standard test conditions.