The band gap values in eV of the prepared CdS thin films as a function of the number of runs and deposition time.

CdS films1 min5 min15 min

1 run2.622.442.45
2 runs2.492.432.44
3 runs2.452.422.43
4 runs2.432.422.42
5 runs2.422.412.42