Light parameters of samples before and after the 24-hour thermal cycle.

SampleExperimental condition (%)FF (%) (mA/cm2) (mV)

1Before10.1059.0123.60725
After8. 4155.3423.16656

2Before11.6063.4424.12758
After10.2159.5923.81721

3Before10.8962.6224.13721
After9.9059.1323.80703