Research Article

H2O/O2 Vapor Annealing Effect on Spin Coating Alumina Thin Films for Passivation of Silicon Solar Cells

Figure 4

Effective carrier lifetime comparison of Al-acac-coated silicon wafers after annealing in different ambients (H2O/O2, O2, and air) for 15 or 120 min at 450°C.