Research Article

Comparison of Photoelectrochemical Current in Amorphous and Crystalline Anodized TiO2 Nanotube Electrodes

Table 1

FWHM of XRD peak (101) at different anodization voltages. Samples were anodized at room temperature and annealed at 450°C.

Anodization voltage (V)FWHM (°)

300.38
400.44
500.58