Research Article
Simulation of the Residual Stress of the Y2O3/Al2O3 Composite Deuterium Permeation Barrier under Thermal Shock
Figure 6
Comparison of the max principal stress in 3 systems of the same individual thickness: (a) max principal stress in Al2O3 coating (); (b) max principal stress in Y2O3 coating (); (c) max principal stress in Y2O3/Al2O3 (150 nm) coating ().
(a) Al2O3, |
(b) Y2O3, |
(c) Y2O3/Al2O3 (150 nm), |