Investigation on Mechanical Properties of GH4720Li at High Strain Rates at Wider Temperature Range

Figure 4

XRD patterns of GH4720Li superalloy under different conditions: (a) 10 s-1, 20°C; (b) 10 s-1, 800°C; (c) 1000 s-1, 20°C; (d) 1000 s-1, 800°C; (e) 5000 s-1, 20°C; (f) 5000 s-1, 800°C.
(a)
(b)
(c)
(d)
(e)
(f)