International Journal of Polymer Science / 2011 / Article / Fig 2

Research Article

Protection of Flax/PLLA Biocomposites from Seawater Ageing by External Layers of PLLA

Figure 2

Effect of different PLLA protective layer thickness on biocomposite water uptake at 40°C.
235805.fig.002

We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.