International Journal of Polymer Science / 2011 / Article / Fig 7

Research Article

Protection of Flax/PLLA Biocomposites from Seawater Ageing by External Layers of PLLA

Figure 7

Damage mechanism of aged samples after 3 months at 40°C. Arrows show damage on the protective layer.
235805.fig.007a
(a)
235805.fig.007b
(b)
235805.fig.007c
(c)

We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.