Research Article

Post-Heat Treatment and Mechanical Assessment of Polyvinyl Alcohol Nanofiber Sheet Fabricated by Electrospinning Technique

Figure 1

Typical SEM micrographs of the PVA electrospun nanofibers: (a) as spun; (b) heat treated at (85°C, which is ~0.5 ); and (c) heat treated at ~1.65 (140°C, which is ~0.7 ).
605938.fig.001a
(a)
605938.fig.001b
(b)
605938.fig.001c