Towards a Smart Encapsulation System for Small-Sized Electronic Devices: A New Approach

Table 3

Measured thickness and calculated NaCl release of selected specimen blends.

Measured parameterSpecimen composition
PVC (m)*   
 (70 : 30)   
(NaCl : PVC)
PS (m)* 
(65 : 30)
(NaCl : PS)
L 210 (m)* 
(40 : 60)
(NaCl : PLA)
L 210 (p)* 
(70 : 30)
(NaCl : PLA)
RG 504 (p)* 
(70 : 30)
(NaCl : PLGA)

Mean release of NaCl compound (%)10092859296
SD of mean released NaCl compound (%)1.740.916.900.890.50
Mean thickness (mm)2.302.603.182.562.51
SD of mean thickness (mm)0.050.160.020.030.30

(m) = mixed manually/(p) = precipitated.