Research Article
Synthesis and Characterization of Chemically Cross-Linked Acrylic Acid/Gelatin Hydrogels: Effect of pH and Composition on Swelling and Drug Release
Table 5
Flory-Huggins network parameters of AA/Gelatin hydrogel.
| Sample codes | Degree of cross-linking (EGDMA) wt % | | | | | | (cm²sec−1) |
| U1 | 0.70 | 0.059 | −0.520 | 949.945 | 106.527 | 8.917 | 0.2289 | U2 | 0.70 | 0.064 | −0.522 | 856.917 | 113.876 | 7.524 | 0.3038 | U3 | 0.70 | 0.065 | −0.522 | 858.763 | 120.869 | 7.105 | 0.3526 | U4 | 0.70 | 0.064 | −0.527 | 918.091 | 130.723 | 7.023 | 0.3316 | U5 | 0.70 | 0.053 | −0.518 | 1245.87 | 124.633 | 9.996 | 0.1559 | U6 | 0.70 | 0.052 | −0.515 | 1291.54 | 119.702 | 10.79 | 0.1487 | U7 | 0.65 | 0.049 | −0.516 | 1483.83 | 120.811 | 12.28 | 0.1301 | U8 | 0.75 | 0.066 | −0.523 | 1031.95 | 120.878 | 8.532 | 0.2547 | U9 | 0.85 | 0.067 | −0.523 | 804.943 | 120.949 | 6.659 | 0.4384 |
|
|