Research Article

Bond Characteristics of Macro Polypropylene Fiber in Cementitious Composites Containing Nanosilica and Styrene Butadiene Latex Polymer

Table 2

Physical properties of cement.

Surface area (cm2/g)Density (g/mm3)Stability (%)Setting timeCompressive strength (MPa)
Initial (min)Final (min)3 days7 days28 days

3,2003.150.02220400203038