Research Article

Tensile Behavior of Polyetheretherketone over a Wide Range of Strain Rates

Figure 6

Deformation process during a 0.001/s strain rate experiment at (a) 19 s, (b) 191 s, (c) 530 s, and (d) 1581 s.
(a)
(b)
(c)
(d)