Water Absorption Behaviour and Its Effect on the Mechanical Properties of Flax Fibre Reinforced Bioepoxy Composites
Table 2
Comparison of the properties of flax and glass fibre.
| Fibre | Density (g/cm3) | Elongation at break (%) | Tensile strength (MPa) | Tensile modulus (GPa) |
| Flax | 1.5 | 2.7–3.2 | 500–900 | 50–70 | E-glass | 2.5 | 2.5 | 2000–3500 | 70 |
|
|