Research Article
Recycling of Cooking Oil Waste into Reactive Polyurethane for Blending with Thermoplastic Polyethylene
Table 1
Thermal property of BP sample.
| Samples | BP |
| First decomposition [°C] | 238 | [°C] | 94 | [°C] | 283 | Weight loss [%] | 19.5% | Second decomposition [°C] | 419 | [°C] | 283 | [°C] | 494 | Weight loss [%] | 57.4% | Third decomposition [°C] | 567 | [°C] | 494 | [°C] | 678 | Weight loss [%] | 16.8% |
|
|