Research Article
Mechanical Behavior and Chloride Penetration of Precracked Reinforced Concrete Beams with Externally Bonded CFRP Exposed to Marine Environment
| Series | Damaged status | Strengthening status | Environmental status and age | Number of specimens |
| C | / | / | / | 3 | D | Damaged | / | / | 2 | F | / | Strengthened | / | 3 | DF | Damaged | Strengthened | / | 4 | FH-3 | / | Strengthened | Exposed for 3 months | 1 | FH-6 | / | Strengthened | Exposed for 6 months | 1 | DFH-3 | Damaged | Strengthened | Exposed for 3 months | 2 | DFH-6 | Damaged | Strengthened | Exposed for 6 months | 3 |
|
|