Temperatures for the thermal degradation of PLLA and PLLA nanocomposites.
| Sample | (°C) | (°C) | (°C) |
| PLLA | 246 | 277 | 301 | PLLA/(1 wt% of Zn/Al palmitate) | 281 | 308 | 352 | PLLA/(2 wt% of Zn/Al palmitate) | 251 | 286 | 323 | PLLA/(1 wt% of LHS (salicylate)) | 249 | 281 | 308 | PLLA/(2 wt% of LHS (salicylate)) | 233 | 269 | 301 | PLLA/(1 wt% of LHS (palmitate)) | 249 | 280 | 318 | PLLA/(2 wt% of LHS (palmitate)) | 242 | 272 | 301 |
|
|