Research Article
UV Dose Governs UV-Polymerized Polyacrylamide Hydrogel Modulus
Figure 3
Young’s modulus as a function of UV exposure time for (a) A12-B.25 and (b) A8-B.10, PAA hydrogels. Asterisks designate significant differences from Young’s modulus for gels polymerized at an exposure time of 300 s (, ).