Degradation temperature (in °C) of composites types A1, B2, and D2.

CompositesTemperature at 10% weight loss (°C)Temperature at 15% weight loss (°C)Temperature at 25% weight loss (°C)Temperature at 50% weight loss (°C)

A1456.52462.48469.74479.60
B2422.11450.39464.64478.01
D2431.32451.88464.96478.52